Series:Composite Piezoelectric Ceramics
Applications:ultrasonic detectors and NDT etc.
Composite Piezoelectric Ceramics
Since the acoustic impedance of the piezoelectric ceramic is greatly different from that of the air, water, or organism, the acoustic wave is difficult to be incident. In order to solve this problem, various resins are compounded with the piezoelectric ceramic. After the composite, piezoceramic acoustic impedance is low, with good incident characteristics, and piezoelectric properties can be adjusted by the volume ratio of ceramic.
Main Applications and Parameters
Non-destructive Inspection
Medical Ultrasonic Detector
Long Distance Ultrasonic Transmitting and Receiving in Solid
Part Number | HTCT |
External Diameter | φ6~φ70mm |
Length | 10~80mm |
Width | 10~30mm |
Thickness | 1~15mm |
Electrode Material | silver/copper/gold |
Recommended Material | P-679.P-672.P-666 |
Electrical Data | Symbol | Main Materials | |||||||||||||
P-659 | P-660 | P-663 | P-664 | P-666 | P-667 | P-668 | P-669 | P-672 | P-673 | P-676 | P-678 | P-679 | P-690 | ||
Piezoelectric coupling coefficien | kp | 0.58 | 0.70 | 0.67 | 0.67 | 0.78 | 0.10 | 0.68 | 0.62 | 0.70 | 0.68 | 0.7 | 0.72 | 0.65 | 0.74 |
k31 | 0.32 | 0.39 | 0.38 | 0.37 | 0.42 | 0.39 | 0.35 | 0.41 | 0.39 | 0.45 | 0.42 | 0.38 | 0.40 | ||
k33 | 0.60 | 0.73 | 0.70 | 0.70 | 0.78 | 0.70 | 0.68 | 0.72 | 0.70 | 0.80 | 0.72 | 0.70 | 0.75 | ||
kt | 0.42 | 0.46 | 0.45 | 0.45 | 0.50 | 0.45 | 0.46 | 0.44 | 0.46 | 0.46 | 0.50 | 0.47 | 0.46 | 0.48 | |
Relative dielectric constant | εT33 / ε0 | 1100 | 3200 | 2200 | 2800 | 4500 | 180 | 2300 | 1400 | 3400 | 2200 | 6000 | 2750 | 1600 | 3800 |
Piezoelectric charge constant | d33×10-12C/N | 280 | 700 | 400 | 480 | 780 | 70 | 430 | 250 | 600 | 430 | 850 | 540 | 320 | 710 |
d31×10-12C/N | -120 | -350 | -200 | -350 | -230 | -130 | -280 | -230 | -420 | -260 | -150 | -360 | |||
Mechanical quality factor | Qm | 100 | 60 | 80 | 500 | 60 | 2500 | 90 | 1000 | 80 | 90 | 60 | 80 | 1000 | 70 |
Frequency constant | fr·d kHz·cm | 230 | 190 | 200 | 220 | 180 | 200 | 230 | 190 | 200 | 180 | 190 | 230 | 190 | |
fr·t kHz·cm | 210 | 200 | 200 | 225 | 200 | 225 | 200 | 200 | |||||||
Temperature characteristics | | TKfr | (-20℃~80℃) | 100 | 260 | 300 | 120 | 400 | 30 | 150 | 100 | 300 | 100 | 400 | 200 | 100 | 260 |
| TKCT | (-20℃~80℃) | 1500 | 4500 | 5000 | 2500 | 6000 | 1800 | 1500 | 4000 | 2000 | 6000 | 3000 | 1500 | 4000 | ||
Curie temperature | Tc | 320 | 220 | 220 | 230 | 180 | 450 | 355 | 340 | 230 | 325 | 140 | 280 | 330 | 210 |
Dielectric loss | tgδ(%) | 1.20 | 1.80 | 2.00 | 0.50 | 2.60 | 0.70 | 2.00 | 0.30 | 2.30 | 2.00 | 2.60 | 1.50 | 0.40 | 1.80 |
Dielectric loss | tgδ(400V/mm,%) | 1.00 | 1.00 |